Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® R 3000 - (TPU-ARES)-GF - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® R 3000:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
DESCRIPTION
Elastollan R 3000 is a glass fibre-reinforced TPU

SPECIAL PROPERTIES
very good impact strength, high stiffness combined with good
strain, low thermal expansion coefficient
equivalent to metal (Al), low mould shrinkage, ease of paintability

TYPICAL APPLICATIONS
technical parts, support of catalyst for plugs, cabinets

OTHER HINTS
predrying: 2-3h at 100-120°C
(air circulating oven or dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
机械性能价值单位Test Standard
ISO数据
拉伸模量 2800 MPa ISO 527
断裂应力 80 MPa ISO 527
断裂伸长率 10 % ISO 527
无缺口简支梁冲击强度, +23°C 120 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 70 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 22 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 10 kJ/m² ISO 179/1eA
断裂应力 TPE 80 MPa ISO 527
断裂应变 TPE 10 % ISO 527
肖氏硬度D 73 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 132 °C ISO 75-1/-2
热变形温度, 0.45 MPa 175 °C ISO 75-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
介质损耗因子, 100Hz 360 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 490 E-4 IEC 62631-2-1
体积电阻率 1E11 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 36 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 1 % 类似ISO 62
密度 1380 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 230 °C ISO 294
注塑, 模具温度 60 °C ISO 294
函数
动态剪切模量-温度 , Elastollan® R 3000, (TPU-ARES)-GF, BASF PU
应力-应变(等时的) 23°C, Elastollan® R 3000, (TPU-ARES)-GF, BASF PU
蠕变模量-时间. 23°C, Elastollan® R 3000, (TPU-ARES)-GF, BASF PU
蠕变曲线 23°C, Elastollan® R 3000, (TPU-ARES)-GF, BASF PU
典型数据
加工方法
注塑
供货形式
粒料
地区供应
其他信息
注塑成型
Barrel temperature : 225 - 235 °C
Melt temperature : 235 °C
Mold temperature: 25 - 70 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.