Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Evoprene® Super G 622 - TPE - Alphagary

Material Data Center offers the following functions for Evoprene® Super G 622:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Evoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
机械性能价值单位Test Standard
ISO数据
拉伸强度 9.4 MPa ISO 37
断裂伸长率 531 % ISO 37
70°C时恒定应变下的永久变形, 24h 34 % ISO 815
100°C时恒定应变下的永久变形, 24h 50 % ISO 815
肖氏硬度A 76 - ISO 7619-1
Other Standards[S]
100%应变时的应力 3.1 MPa ISO 37
300%应变时的应力 16.8 MPa ISO 37
撕裂强度 40 kN/m ISO 6383
耐磨性 181 mm³ DIN 53516
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
ISO数据
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 6.0 mm -
燃烧性-氧指数 26 % ISO 4589-1/-2
其它性能价值单位Test Standard
Other Standards[S]
密度 1140 kg/m³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
典型数据
加工方法
注塑
地区供应
北美, 欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.