Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HOSTAFORM® C 2521 XAP®2 - POM - Celanese

Material Data Center offers the following functions for HOSTAFORM® C 2521 XAP®2:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Hostaform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 2.5 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
熔体密度 1200 kg/m³ -
熔体 0.155 W/(m K) -
熔体的比热 2210 J/(kg K) -
喷射温度 140 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2450 MPa ISO 527
屈服应力 62 MPa ISO 527
屈服伸长率 9 % ISO 527
名义断裂伸长率 35 % ISO 527
无缺口简支梁冲击强度, +23°C 250 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 250 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 8.5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 7 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 166 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 101 °C ISO 75-1/-2
线性热膨胀系数, 平行 120 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 120 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 4 - IEC 62631-2-1
相对介电常数., 1MHz 4 - IEC 62631-2-1
介质损耗因子, 100Hz 15 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 50 E-4 IEC 62631-2-1
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 35 kV/mm IEC 60243-1
其它性能价值单位Test Standard
吸水性 0.65 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1410 kg/m³ ISO 1183
函数
粘度-剪切速度 , HOSTAFORM® C 2521 XAP®2, POM, Celanese
剪切应力-剪切速度 , HOSTAFORM® C 2521 XAP®2, POM, Celanese
动态剪切模量-温度 , HOSTAFORM® C 2521 XAP®2, POM, Celanese
应力-应变.  , HOSTAFORM® C 2521 XAP®2, POM, Celanese
正割模量-应变.  , HOSTAFORM® C 2521 XAP®2, POM, Celanese
应力-应变(等时的) 23°C, HOSTAFORM® C 2521 XAP®2, POM, Celanese
蠕变模量-时间. 23°C, HOSTAFORM® C 2521 XAP®2, POM, Celanese
蠕变曲线 23°C, HOSTAFORM® C 2521 XAP®2, POM, Celanese
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 吹塑
供货形式
粒料
添加剂
脱模助剂
特征
共聚物
其他信息
注塑成型
To achive low emission values pre drying using a recirculating air dryer (100 to 120 °C / max. 40 mm layer / 3 to 6 hours) is recommended.

Max. Water content 0,1 %
Standard injection moulding machines with three phase (15 to 25 D)
plasticating screws will fit.

Conditioning e.g. moisturizing is not necessary.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.