Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hybrid S555 - (PC+ABS) - Ravago Manufacturing Americas

Material Data Center offers the following functions for Hybrid S555:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hybrid S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 24 cm³/10min ISO 1133
温度 260 °C -
载荷 2.16 kg -
模塑收缩率, 平行 0.6 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 21 g/10min ASTM D 1238
温度 260 °C -
负载 2.16 kg -
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
屈服应力 62 MPa ISO 527
断裂伸长率 48 % ISO 527
弯曲模量, 23°C 2550 MPa ISO 178
悬臂梁缺口冲击强度, +23°C 44 kJ/m² ISO 180/1A
ASTM数据
屈服应力 63.4 MPa ASTM D 638
断裂伸长率 45 % ASTM D 638
弯曲模量 2550 MPa ASTM D 790
弯曲强度 84.1 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 640 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 91 °C ISO 75-1/-2
热变形温度, 0.45 MPa 105 °C ISO 75-1/-2
厚度为h时的5V燃烧性 5VB class IEC 60695-11-20
测试用试样的厚度 2.5 mm -
ASTM数据
UL94 燃烧性 V-0 - UL 94
测试厚度 1.5 mm -
DTUL @ 66 psi 107 °C ASTM D 648
DTUL @ 264 psi 93.9 °C ASTM D 648
维卡温度 110 °C ASTM D 1525
其它性能价值单位Test Standard
密度 1180 kg/m³ ISO 1183
密度 1180 kg/m³ ASTM D 792
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
阻燃的
地区供应
北美
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com