Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR53 - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR53:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
K-Resin® KR53 makes a clear, stiff, very tough, high gloss film suitable for applications such as candy twist wrap, shrink sleeves and overwrap.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 10 cm³/10min ISO 1133
温度 200 °C -
载荷 5 kg -
熔融指数, MFI 10 g/10min ISO 1133
温度 200 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 650 MPa ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 8 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
维卡软化温度, B 40 °C ISO 306
ASTM数据
维卡温度 63 °C ASTM D 1525
光学特性价值单位Test Standard
ASTM数据
光泽度 140 - ASTM D 2457
雾度 0.2 % ASTM D 1003
其它性能价值单位Test Standard
吸湿性 0.07 % 类似ISO 62
密度 1010 kg/m³ ISO 1183
机械性能(薄膜)价值单位Test Standard
ISO数据
最大应变, 平行 175 % ISO 527-3
最大应变, normal 180 % ISO 527-3
挤出形式 麓碌陇 - -
试样厚度 0.025 mm -
ASTM Data
屈服应力, 平行 25 MPa ASTM D 882
屈服应力, 垂直 20 MPa ASTM D 882
挤出形式 麓碌陇 - -
试样厚度 0.025 mm -
典型数据
加工方法
吹塑挤出成型, 薄膜挤出成型
供货形式
粒料
特殊性能
透明.
特征
可热封的, High Gloss, 共聚物
应用
药物, 包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.