Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KEYFLEX BT 1245D - TPC - LG Chem

Material Data Center offers the following functions for KEYFLEX BT 1245D:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Keyflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 25 g/10min ASTM D 1238
温度 220 °C -
负载 2.16 kg -
模压收缩率, 平行 0.016 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
断裂拉伸强度 29.4 MPa ASTM D 638
断裂伸长率 600 % ASTM D 638
弯曲模量 98.1 MPa ASTM D 790
邵氏硬度D 44 - ASTM D 2240
悬臂梁缺口冲击强度, 1/4 in N J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature N J/m ASTM D 256
温度 -40 °C -
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 60 °C ASTM D 648
熔点 205 °C ASTM D 3418
电性能价值单位Test Standard
ISO数据
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水率, 24小时 0.6 % ASTM D 570
密度 1130 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 90 °C -
预干燥-时间 3 - 4 h -
加工湿度 ≤0.01 % -
注塑熔体温度 205 - 235 °C -
模具温度 10 - 35 °C -
1区 205 - 225 °C -
2区 210 - 230 °C -
3区 215 - 235 °C -
喷嘴温度 215 - 235 °C -
典型数据
加工方法
注塑, 其它挤出成型
供货形式
黑色
应用
汽车
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.