Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KIBISAN PN-127H - SAN - CHIMEI Corporation

Material Data Center offers the following functions for KIBISAN PN-127H:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kibisan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 18 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
ASTM数据
熔融指数, MFI 1.5 g/10min ASTM D 1238
温度 200 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
屈服应力 79 MPa ISO 527
断裂应力 79 MPa ISO 527
弯曲模量, 23°C 3600 MPa ISO 178
弯曲强度 109 MPa ISO 178
简支梁缺口冲击强度, +23°C 3 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C 3 kJ/m² ISO 180/1A
ASTM数据
屈服应力 76.5 MPa ASTM D 638
弯曲模量 3585 MPa ASTM D 790
弯曲强度 108 MPa ASTM D 790
洛克硬度 M 85 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 22.4 J/m ASTM D 256
悬臂梁缺口冲击强度, 1/4 in 18.7 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 91 °C ISO 75-1/-2
维卡软化温度, A 107 °C ISO 306
维卡软化温度, B 104 °C ISO 306
线性热膨胀系数, 平行 37 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.59 mm -
维卡温度 107 °C ASTM D 1525
其它性能价值单位Test Standard
密度 1060 kg/m³ ISO 1183
密度 1060 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 75 - 80 °C -
预干燥-时间 3 - 4 h -
模具温度 40 - 60 °C -
加料温度 190 - 210 °C -
1区 200 - 220 °C -
喷嘴温度 200 - 220 °C -
注射压力 5 - 7 MPa -
背压 0.5 - 1.5 MPa -
保压压力 4 - 6 MPa -
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的
耐化学试剂
通用耐化学性
Certifications
RoHS
应用
电子电气
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.