Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDG1033R - PA66-GF30 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDG1033R:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.005 mm/mm ASTM D 955
模压收缩率, TD 0.007 mm/mm ASTM D 955
机械性能干 / 已调节单位Test Standard
ISO数据
简支梁冲击强度, +23°C 95 / 100 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 13.5 / 18.5 kJ/m² ISO 179/1eA
ASTM数据
拉伸模量 11000 / 8500 MPa ASTM D 638
拉伸强度 200 / 145 MPa ASTM D 638
弯曲模量 9500 / 6500 MPa ASTM D 790
弯曲强度 270 / 190 MPa ASTM D 790
洛克硬度 R 120 / R 115 - ASTM D 785
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 HB - UL 94
热释放速率, 平行 22 E-6/K ASTM D 696
DTUL @ 66 psi 260 °C ASTM D 648
DTUL @ 264 psi 260 °C ASTM D 648
熔点 260 °C ASTM D 3418
电性能干 / 已调节单位Test Standard
ASTM数据
电介质强度, 短时 34 / - kV/mm ASTM D 149
耗散因素, 1 MHz 0.01 / - - ASTM D 150
电介质常数, 1 MHz 3.7 / - - ASTM D 150
体积电阻率 1E15 / - Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水率, 24小时 0.75 % ASTM D 570
密度 1390 kg/m³ ASTM D 792
典型数据
特殊性能
经热稳处理的/耐热的
应用
汽车, 电子电气
地区供应
北美, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.