Any use of this information falls under the rules of our
disclaimer.
材料文字说明
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of
poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance
from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For Molding, Compound, Additives.
加工/物理特性 | 价值 | 单位 | Test Standard |
ISO数据 |
熔融指数, MFI |
4.8 |
g/10min |
ISO 1133 |
温度 |
190 |
°C |
- |
负载 |
2.16 |
kg |
- |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
简支梁缺口冲击强度, +23°C |
N |
kJ/m² |
ISO 179/1eA |
拉伸强度 |
15 |
MPa |
ISO 37 |
肖氏硬度A |
68 |
- |
ISO 7619-1 |
肖氏硬度D |
22 |
- |
ISO 7619-1 |
Other Standards[S] |
100%应变时的应力 |
9.3 |
MPa |
ISO 37 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
热性能 | 价值 | 单位 | Test Standard |
Other Standards[S] |
热导率, 固态 |
0.15 |
W/(m K) |
ASTM E 1530 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
电性能 | 价值 | 单位 | Test Standard |
Other Standards[S] |
耗散因素, 60 Hz |
0.0288 |
- |
JIS C 2138 |
耗散因素, 1 MHz |
0.0552 |
- |
JIS C 2138 |
电介质常数, 60 Hz |
4.84 |
- |
JIS C 2138 |
电介质常数, 1 MHz |
3.97 |
- |
JIS C 2138 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
光学特性 | 价值 | 单位 | Test Standard |
ISO Data |
浑浊率 |
2 |
- |
ISO 14782 |
Other Standards[S] |
光透射率 |
93 |
% |
ISO 13468-1 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
其它性能 | 价值 | 单位 | Test Standard |
密度 |
1100 |
kg/m³ |
ISO 1183 |
加工推荐(挤出) | 价值 | 单位 | Test Standard |
加料温度 |
100 - 130 |
°C |
- |
1区 |
140 - 160 |
°C |
- |
2区 |
150 - 170 |
°C |
- |
喷嘴温度 |
150 - 170 |
°C |
- |
典型数据
加工方法
其它挤出成型
供货形式
粒料
特殊性能
经耐紫外线处理的/耐气候的, 透明.
特征
共混树脂, 少气味, 共聚物
耐化学试剂
耐酸性, 耐碱性, 耐油性
应用
汽车, 电子电气
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.