Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kurarity™ LA2270 - TPE - Kuraray Co., Ltd.

Material Data Center offers the following functions for Kurarity™ LA2270:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kurarity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For Molding, Compound, Additives.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 4.8 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
简支梁缺口冲击强度, +23°C N kJ/m² ISO 179/1eA
拉伸强度 15 MPa ISO 37
肖氏硬度A 68 - ISO 7619-1
肖氏硬度D 22 - ISO 7619-1
Other Standards[S]
100%应变时的应力 9.3 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
Other Standards[S]
热导率, 固态 0.15 W/(m K) ASTM E 1530
S: These properties are reported by the producer according standards that are different to our defaults.
电性能价值单位Test Standard
Other Standards[S]
耗散因素, 60 Hz 0.0288 - JIS C 2138
耗散因素, 1 MHz 0.0552 - JIS C 2138
电介质常数, 60 Hz 4.84 - JIS C 2138
电介质常数, 1 MHz 3.97 - JIS C 2138
S: These properties are reported by the producer according standards that are different to our defaults.
光学特性价值单位Test Standard
ISO Data
浑浊率 2 - ISO 14782
Other Standards[S]
光透射率 93 % ISO 13468-1
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
密度 1100 kg/m³ ISO 1183
加工推荐(挤出)价值单位Test Standard
加料温度 100 - 130 °C -
1区 140 - 160 °C -
2区 150 - 170 °C -
喷嘴温度 150 - 170 °C -
典型数据
加工方法
其它挤出成型
供货形式
粒料
特殊性能
经耐紫外线处理的/耐气候的, 透明.
特征
共混树脂, 少气味, 共聚物
耐化学试剂
耐酸性, 耐碱性, 耐油性
应用
汽车, 电子电气
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.