Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar® 710 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar® 710:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar® 710 resin is a grade of granules for injection molding, rotomolding applications and multifilament extrusion. This product is NSF/ANSI/CAN 61 certified. 

A powder form is available as Kynar® 711 resin.


Main applications:
  • corrosion protection in the chemical industry
  • coating (painting, co-extrusion)
  • off shore
  • wire and cable
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 20 cm³/10min ISO 1133
温度 230 °C -
载荷 5 kg -
模塑收缩率, 平行 2.0 % ISO 294-4, 2577
模塑收缩率, 垂直 2.0 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 2300 MPa ISO 527
屈服应力 54 MPa ISO 527
屈服伸长率 9 % ISO 527
名义断裂伸长率 >50 % ISO 527
无缺口简支梁冲击强度, +23°C 192 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 208 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 8 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 168 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -40 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 110 °C ISO 75-1/-2
热变形温度, 0.45 MPa 130 °C ISO 75-1/-2
维卡软化温度, B 140 °C ISO 306
线性热膨胀系数, 平行 150 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
燃烧性-氧指数 43 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 9 - IEC 62631-2-1
相对介电常数., 1MHz 6 - IEC 62631-2-1
介质损耗因子, 100Hz 350 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 2060 E-4 IEC 62631-2-1
体积电阻率 2E12 Ohm*m IEC 62631-3-1
其它性能价值单位Test Standard
吸水性 0.03 % 类似ISO 62
密度 1780 kg/m³ ISO 1183
函数
粘度-剪切速度 , Kynar® 710, PVDF, ARKEMA
剪切应力-剪切速度 , Kynar® 710, PVDF, ARKEMA
应力-应变.  , Kynar® 710, PVDF, ARKEMA
正割模量-应变.  , Kynar® 710, PVDF, ARKEMA
比容-温度(pvT) , Kynar® 710, PVDF, ARKEMA
典型数据
加工方法
注塑, 薄膜挤出成型
供货形式
粒料
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的, 透明.
特征
均聚物
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.