加工/物理特性 | 价值 | 单位 | Test Standard |
ASTM数据 |
熔融指数, MFI |
7 |
g/10min |
ASTM D 1238 |
温度 |
300 |
°C |
- |
负载 |
1.2 |
kg |
- |
模压收缩率, 平行 |
0.006 |
mm/mm |
ASTM D 955 |
机械性能 | 价值 | 单位 | Test Standard |
ASTM数据 |
拉伸模量 |
2410 |
MPa |
ASTM D 638 |
屈服应力 |
60 |
MPa |
ASTM D 638 |
断裂拉伸强度 |
72 |
MPa |
ASTM D 638 |
屈服伸长率 |
6 |
% |
ASTM D 638 |
断裂伸长率 |
150 |
% |
ASTM D 638 |
弯曲模量 |
2410 |
MPa |
ASTM D 790 |
弯曲强度 |
96 |
MPa |
ASTM D 790 |
洛克硬度 |
M 74 |
- |
ASTM D 785 |
悬臂梁缺口冲击强度, 1/8 in |
900 |
J/m |
ASTM D 256 |
Izod冲击强度, 1/8 in |
N |
J/m |
ASTM D 256 |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
厚度为h时的燃烧性 |
HB |
class |
IEC 60695-11-10 |
测试用试样的厚度 |
3.0 |
mm |
- |
Yellow Card 现存 |
是的 |
- |
- |
灼热丝引燃温度 (GWIT) |
850 |
°C |
IEC 60695-2-13 |
GWIT - 测试用试样厚度 |
2 |
mm |
- |
ASTM数据 |
UL94 燃烧性 |
HB |
- |
UL 94 |
测试厚度 |
0.5 |
mm |
- |
热释放速率, 平行 |
68 |
E-6/K |
ASTM D 696 |
DTUL @ 66 psi |
145[ann.] |
°C |
ASTM D 648 |
DTUL @ 264 psi |
129 |
°C |
ASTM D 648 |
维卡温度 |
151 |
°C |
ASTM D 1525 |
氧指数 |
26 |
% |
ASTM D 2863 |
电性能 | 价值 | 单位 | Test Standard |
ISO数据 |
相对漏电起痕指数 |
250 |
- |
IEC 60112 |
ASTM数据 |
电介质强度, 短时 |
17 |
kV/mm |
ASTM D 149 |
耗散因素, 60 Hz |
0.001 |
- |
ASTM D 150 |
电介质常数, 60 Hz |
3 |
- |
ASTM D 150 |
体积电阻率 |
2E17 |
Ohm*cm |
ASTM D 257 |
光学特性 | 价值 | 单位 | Test Standard |
ASTM数据 |
雾度 |
1.1 |
% |
ASTM D 1003 |
光透射率 |
89 |
% |
ASTM D 1003 |
折射率 |
1.59 |
- |
ASTM D 542 |
其它性能 | 价值 | 单位 | Test Standard |
吸水率, 24小时 |
0.15 |
% |
ASTM D 570 |
吸水率, 平衡 |
0.32 |
% |
ASTM D 570 |
密度 |
1200 |
kg/m³ |
ASTM D 792 |
典型数据
加工方法
注塑, 片材挤出成型, 其它挤出成型
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的, 透明.
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.