Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® AX2675 ST - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® AX2675 ST:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
  • Automotive eXterior grade with specified Sensor signal Transparency
  • MVR (300 °C/1.2 kg) 12 cm³/10 min
  • medium viscosity
  • easy release
  • developed for high-gloss surfaces with highest requirements
  • for the use in combination with hard coatings
  • for high transmittance applications in the near-infrared range (NIR)
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 12 cm³/10min ISO 1133
温度 300 °C -
载荷 1.2 kg -
熔融指数, MFI 13 g/10min ISO 1133
温度 300 °C -
负载 1.2 kg -
模塑收缩率, 平行 0.7 % ISO 294-4, 2577
模塑收缩率, 垂直 0.8 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 2400 MPa ISO 527
屈服应力 65 MPa ISO 527
屈服伸长率 6 % ISO 527
名义断裂伸长率 >50 % ISO 527
弯曲模量, 23°C 2400 MPa ISO 178
弯曲强度 98 MPa ISO 178
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, 3mm 70 kJ/m² ISO 179/1eA
Type of failure P - -
简支梁缺口冲击强度, -30°C, 3mm 16 kJ/m² ISO 179/1eA
Type of failure C - -
悬臂梁缺口冲击强度, +23°C 70 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 14 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -30 °C -
冲孔最大力, +23°C 5200 N ISO 6603-2
冲孔最大力, -30°C 6100 N ISO 6603-2
冲孔功, +23°C 55 J ISO 6603-2
冲孔功, -30°C 60 J ISO 6603-2
球压硬度 115 MPa ISO 2039-1
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 143 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 124 °C ISO 75-1/-2
热变形温度, 0.45 MPa 136 °C ISO 75-1/-2
维卡软化温度, B 143 °C ISO 306
线性热膨胀系数, 平行 65 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 65 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.1 - IEC 62631-2-1
相对介电常数., 1MHz 3 - IEC 62631-2-1
介质损耗因子, 100Hz 5 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 90 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 34 kV/mm IEC 60243-1
相对漏电起痕指数 250 - IEC 60112
光学特性价值单位Test Standard
ISO Data
透光率 89 % ISO 13468-1, -2
其它性能价值单位Test Standard
吸水性 0.3 % 类似ISO 62
吸湿性 0.12 % 类似ISO 62
密度 1200 kg/m³ ISO 1183
Bulk density 660 kg/m³ -
机械性能(薄膜)价值单位Test Standard
ISO数据
下水蒸汽透过率, 23°C/85%RH 15 g/(m²*d) ISO 15106-1/-2
试样厚度 0.1 mm -
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 290 °C ISO 294
注塑, 模具温度 80 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 120 °C -
预干燥-时间 4 h -
加工湿度 ≤0.02 % -
注塑熔体温度 280 - 320 °C -
模具温度 70 - 110 °C -
1区 250 - 270 °C -
2区 270 - 290 °C -
3区 285 - 305 °C -
喷嘴温度 270 - 305 °C -
背压 5 - 15 MPa -
典型数据
加工方法
注塑
供货形式
粒料, 黑色
添加剂
脱模助剂
特征
High Gloss
应用
汽车
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.