Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MELOCHEM -791 Grade - MF-L - Chemiplastica

Material Data Center offers the following functions for MELOCHEM -791 Grade:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Melochem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.7 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸强度 45 MPa ISO 527
简支梁冲击强度, +23°C 5 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 1.1 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 8.00 MPa 110 °C ISO 75-1/-2
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
ASTM数据
氧指数 40 % ASTM D 2863
电性能价值单位Test Standard
ISO数据
表面电阻率 1E10 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
密度 1500 kg/m³ ISO 1183
典型数据
加工方法
模压成型
供货形式
粉料
添加剂
润滑剂
特殊性能
经光稳处理的/耐光的
特征
少气味, 抗划性
耐化学试剂
通用耐化学性, 耐油性
Certifications
生物相容
应用
电子电气
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.