Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NILAC F28 - ABS-GF28 - Soredi S.p.a.

Material Data Center offers the following functions for NILAC F28:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Nilac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 5 g/10min ASTM D 1238
温度 220 °C -
负载 10 kg -
模压收缩率, 平行 0.003 mm/mm ASTM D 955
模压收缩率, TD 0.004 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
断裂拉伸强度 70 MPa ASTM D 638
弯曲模量 7500 MPa ASTM D 790
弯曲强度 100 MPa ASTM D 790
洛克硬度 R 115 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 62.5 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 48 J/m ASTM D 256
温度 -20 °C -
热性能价值单位Test Standard
ISO数据
线性热膨胀系数, 垂直 30 E-6/K ISO 11359-1/-2
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.6 mm -
DTUL @ 264 psi 104 °C ASTM D 648
维卡温度 108 °C ASTM D 1525
电性能价值单位Test Standard
ISO数据
相对介电常数, 1MHz 2.8 - IEC 62631-2-1
介质损耗因子, 1MHz 100 E-4 IEC 62631-2-1
体积电阻率 1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E15 Ohm IEC 62631-3-2
介电强度 30 kV/mm IEC 60243-1
其它性能价值单位Test Standard
吸湿性 0.2 % 类似ISO 62
密度 1250 kg/m³ ASTM D 792
典型数据
加工方法
注塑
供货形式
自然色
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.