Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F30 AGR HF - PP-GF30 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F30 AGR HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 10 g/10min ASTM D 1238
温度 230 °C -
负载 2.16 kg -
模压收缩率, 平行 0.004 mm/mm ASTM D 955
模压收缩率, TD 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
断裂拉伸强度 90 MPa ASTM D 638
弯曲模量 6000 MPa ASTM D 790
弯曲强度 140 MPa ASTM D 790
洛克硬度 R 113 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 125 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 76.9 J/m ASTM D 256
温度 -20 °C -
热性能价值单位Test Standard
ISO数据
线性热膨胀系数, 垂直 30 E-6/K ISO 11359-1/-2
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.6 mm -
DTUL @ 264 psi 153 °C ASTM D 648
维卡温度 144 °C ASTM D 1525
电性能价值单位Test Standard
ISO数据
相对介电常数, 1MHz 2.7 - IEC 62631-2-1
体积电阻率 1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 60 kV/mm IEC 60243-1
其它性能价值单位Test Standard
吸湿性 0.1 % 类似ISO 62
密度 1120 kg/m³ ASTM D 792
典型数据
特征
化学偶合增强, 均聚物
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com