Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® Ultra 4105 - (ABS+PC) - INEOS Styrolution

Material Data Center offers the following functions for Novodur® Ultra 4105:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Novodur® Ultra 4105 acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® Ultra 4105 is a PC modified high heat injection molding grade with very high impact strength. Furthermore, it is of low emission, i.e. suitable to produce parts which fulfill interior emission requirements of the automotive OEMs.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 14 cm³/10min ISO 1133
温度 260 °C -
载荷 5 kg -
熔体密度 972 kg/m³ -
熔体 0.232 W/(m K) -
熔体的比热 2330 J/(kg K) -
喷射温度 94 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2000 MPa ISO 527
屈服应力 45 MPa ISO 527
屈服伸长率 3.7 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 40 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 32 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 99 °C ISO 75-1/-2
热变形温度, 0.45 MPa 108 °C ISO 75-1/-2
维卡软化温度, B 107 °C ISO 306
线性热膨胀系数, 平行 90 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
介电强度 37 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
密度 1070 kg/m³ ISO 1183
函数
粘度-剪切速度 , Novodur® Ultra 4105, (ABS+PC), INEOS Styrolution
剪切应力-剪切速度 , Novodur® Ultra 4105, (ABS+PC), INEOS Styrolution
典型数据
加工方法
注塑
供货形式
粒料
特征
低排放
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 230 - 260°C

Mold temperature, range: 60 - 80°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.