Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2507F Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2507F Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Platamid® HX 2507F Pellets
Alcohol Soluble Copolyamides

Platamid® HX 2507F Alcohol Soluble Copolyamides comprises copolyamides of different structures, molecular weights and melting characteristics which are particularly well suited for coating solutions. The products offer good film forming properties, excellent abrasion resistance and good adhesion to both metallic and non-metallic surfaces. 

The main feature of all products us the ability to form stable solutions after dissolving in lower aliphatic alcohols, such as:
  • Methanol
  • Ethanol
  • Propanol / Isopropanol
  • Butanol / Isobutanol
  • or mixtures of these 

As well as in higher boiling alcohols, such as:
  • Benzyl alcohol
  • cyclohexanol
Aromatic hydrocarbons, like xylene, or SOLVESSO®, can be added at concentrations up to 20 to 30 parts by weight. These hydrocarbons do not interfere with dissolution, and improve storage stability. Solubility in conventional lacquer solvents such as ketones, esters or ethers is negligible.
All Platamid® grades are compatible in solution. This allows blending to achieve special effects. 


AVAILABLE GRADES

This grade is available:

Non-dried pellets („F“) with a maximum residual moisture content of ≤ 1.8 %

PACKAGING

In 25 kg paper bags with aluminium foil / polyethylene liners on 1000 kg pallets

SHELF LIFE

Two years from the date of delivery. For any use above this limit, please refer to our technical services.



加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 0.6 / * cm³/10min ISO 1133
温度 190 / * °C -
载荷 2.16 / * kg -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 155 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 115 / * °C ISO 11357-1/-2
其它性能干 / 已调节单位Test Standard
吸水性 4.5 / * % 类似ISO 62
密度 992 / 992 kg/m³ ISO 1183
典型数据
加工方法
薄膜挤出成型, 表面涂层
供货形式
粒料
特征
共混树脂, 好粘附性能, 共聚物
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com