Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Polylan ABS 3O 52 - ABS - Polyma Kunststoff GmbH & Co.KG
Material Data Center offers the following functions for Polylan ABS 3O 52:
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Polylan datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
加工/物理特性 | 价值 | 单位 | Test Standard |
Other Standards[S] |
熔融指数, MFI |
20 |
g/10min |
DIN 53735 |
温度 |
220 |
°C |
- |
负载 |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
简支梁缺口冲击强度, +23°C |
10 |
kJ/m² |
ISO 179/1eA |
悬臂梁缺口冲击强度, +23°C |
17 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
拉伸模量 |
2400 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
热性能 | 价值 | 单位 | Test Standard |
Other Standards[S] |
维卡软化温度, B |
95 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
其它性能 | 价值 | 单位 | Test Standard |
Other Standards[S] |
密度 |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.