Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® BF940L - PA* - Nurel S.A.

Material Data Center offers the following functions for Promyde® BF940L:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 18 cm³/10min ISO 1133
温度 275 °C -
载荷 5 kg -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 200 °C ISO 11357-1/-3
光学特性价值单位Test Standard
ASTM数据
雾度 0.5 % ASTM D 1003
其它性能价值单位Test Standard
密度 1110 kg/m³ ISO 1183
Moisture Content 0.1 % -
机械性能(薄膜)价值单位Test Standard
ISO数据
断裂应力, 平行 65 MPa ISO 527-3
最大应变, 平行 400 % ISO 527-3
继续撕裂强度, 平行 30 N/mm ISO 6383-1
动态摩擦系数 0.25 - ISO 8295
下水蒸汽透过率, 23°C/85%RH 20 g/(m²*d) ISO 15106-1/-2
下氧气透过率, 23°C/0%RH 25 cm³/(m²*d*bar) ISO 15105-1/-2
下氧气透过率, 23°C/85%RH 25 cm³/(m²*d*bar) ISO 15105-1/-2
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数. 263 cm³/g ISO 307, 1157, 1628
加工推荐(挤出)价值单位Test Standard
预干燥-温度 75 - 80 °C -
加料温度 40 - 50 °C -
1区 210 - 250 °C -
喷嘴温度 240 - 250 °C -
典型数据
加工方法
吹塑挤出成型, 薄膜挤出成型, 热成型
添加剂
润滑剂
特殊性能
透明.
Certifications
可食品接触的
应用
包装
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com