Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® Clear G850 Rnew® - PA* - ARKEMA

Material Data Center offers the following functions for Rilsan® Clear G850 Rnew®:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
PA,,GHT,C14-020

Rilsan® Clear G850 Rnew® is a high performance transparent copolyamide, partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited for optic as high end eyewear frames.

According to ASTM D6866, the biobased carbon content is measured at 45%.



Main applications:
  • Sun
  • optical
  • reading glass frames
  • Structural frames of smart phones
  • Watch covers
  • Household appliances

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit,  please refer to our technical services.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 4.4 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 2.16 / * kg -
模塑收缩率, 平行 0.9 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.9 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1680 / 1640 MPa ISO 527
屈服应力 64 / 58 MPa ISO 527
屈服伸长率 8.2 / 8.6 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
简支梁缺口冲击强度, +23°C 8.5 / 15 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 8.6 / 11.4 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 145 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 120 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 135 / * °C ISO 75-1/-2
1.5mm名义厚度时的燃烧性 V-2 / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
Yellow Card 现存 是的 / * - -
其它性能干 / 已调节单位Test Standard
吸水性 4 / * % 类似ISO 62
吸湿性 1.7 / * % 类似ISO 62
密度 1010 / 1010 kg/m³ ISO 1183
Biobased content 45 % -
函数
粘度-剪切速度 , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
剪切应力-剪切速度 , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
比容-温度(pvT) , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
典型数据
加工方法
注塑, 薄膜挤出成型
供货形式
粒料
特殊性能
经热稳处理的/耐热的, 透明.
Certifications
生物相容
地区供应
其他信息
注塑成型
Injection Process conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 250°C / 280°C / 300°C
- Typical mold temperature  : 20 - 80 °C
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C
薄膜挤出成型
Extrusion Process conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 250°C / 270°C / 290°C
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.