Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SLOVAMID®6 OB - PA6 - Plastcom, spol. s r.o.

Material Data Center offers the following functions for SLOVAMID®6 OB:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Slovamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 6 g/10min ISO 1133
温度 230 °C -
负载 2.16 kg -
模塑收缩率, 平行 1.4 % ISO 294-4, 2577
模塑收缩率, 垂直 1.4 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 3400 MPa ISO 527
拉伸强度 85 MPa ISO 527
弯曲模量, 23°C 2950 MPa ISO 178
简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 220 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 55 °C ISO 75-1/-2
维卡软化温度, B 190 °C ISO 306
1.5mm名义厚度时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
电性能价值单位Test Standard
ISO数据
介电强度 18 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
密度 1130 kg/m³ ISO 1183
Moisture Content 0.15 % -
典型数据
加工方法
注塑
供货形式
自然色
应用
电子电气
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.