Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styroflex® ECO 2G66 BC60 - SB - INEOS Styrolution

Material Data Center offers the following functions for Styroflex® ECO 2G66 BC60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styroflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 77 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources: 60 %
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 13 cm³/10min ISO 1133
温度 200 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 70 MPa ISO 527
屈服应力 3 MPa ISO 527
屈服伸长率 50 % ISO 527
名义断裂伸长率 500 % ISO 527
断裂应力 9 MPa ISO 527
断裂伸长率 450 % ISO 527
弯曲模量, 23°C 60 MPa ISO 178
弯曲强度 2 MPa ISO 178
简支梁缺口冲击强度, +23°C N kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 2 kJ/m² ISO 179/1eA
肖氏硬度A 86 - ISO 7619-1
肖氏硬度D 30 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
维卡软化温度, A 39 °C ISO 306
光学特性价值单位Test Standard
ASTM数据
雾度 10 % ASTM D 1003
光透射率 80 % ASTM D 1003
Other Standards[S]
折射率 1.57 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
吸水性 0.07 % 类似ISO 62
密度 998 kg/m³ ISO 1183
加工推荐(挤出)价值单位Test Standard
注塑熔体温度 170 - 240 °C -
模具温度 30 - 50 °C -
典型数据
加工方法
注塑, 吹塑挤出成型, 薄膜挤出成型
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的, 透明., 消毒, 环氧乙烷灭菌(EtO), Gamma irradiation sterilization
耐化学试剂
抗辐射性
Certifications
生物相容, 可食品接触的, ISCC Plus
应用
药物, 包装
地区供应
欧洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com