Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPX® MX0020 - PMP - Mitsui Chemicals America, Inc.

Material Data Center offers the following functions for TPX® MX0020:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other TPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 21 g/10min ASTM D 1238
温度 260 °C -
负载 5 kg -
模压收缩率, 平行 1.5 mm/mm ASTM D 955
模压收缩率, TD 1.1 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 882.5 MPa ASTM D 638
拉伸强度 10 MPa ASTM D 638
屈服应力 21 MPa ASTM D 638
断裂伸长率 60 % ASTM D 638
弯曲模量 659.8 MPa ASTM D 790
弯曲强度 27 MPa ASTM D 790
洛克硬度 R42 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 27.8 J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
热释放速率, 平行 380 E-6/K ASTM D 696
DTUL @ 66 psi 92.8 °C ASTM D 648
维卡温度 153 °C ASTM D 1525
电性能价值单位Test Standard
ASTM数据
体积电阻率 1E16 Ohm*cm ASTM D 257
光学特性价值单位Test Standard
ASTM数据
雾度 1.2 % ASTM D 1003
光透射率 93 % ASTM D 1003
折射率 1.46 - ASTM D 542
其它性能价值单位Test Standard
密度 833 kg/m³ ASTM D 792
典型数据
加工方法
注塑, 纤维挤出, 薄膜挤出成型, 其它挤出成型, 吹塑
Certifications
可食品接触的, FDA 21 CFR认证
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.