Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TIPELIN 7000F - (PE-HD) - MOL Petrochemicals Co. Ltd.

Material Data Center offers the following functions for TIPELIN 7000F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tipelin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 0.08 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
弯曲模量, 23°C 1500 MPa ISO 178
肖氏硬度D 64 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
维卡软化温度, A 126 °C ISO 306
其它性能价值单位Test Standard
密度 955 kg/m³ ISO 1183
机械性能(薄膜)价值单位Test Standard
ISO数据
屈服应力, 平行 30 MPa ISO 527-3
屈服应力, normal 24 MPa ISO 527-3
断裂应力, 平行 71 MPa ISO 527-3
断裂应力, 垂直 43 MPa ISO 527-3
最大应变, 平行 500 % ISO 527-3
最大应变, normal 600 % ISO 527-3
埃尔曼多夫撕裂强度, 平行 16 N ISO 6383-2
埃尔曼多夫撕裂强度, 垂直 155 N ISO 6383-2
落镖试验A 200 g ISO 7765-1
挤出形式 麓碌陇 - -
试样厚度 0.015 mm -
加工推荐(挤出)价值单位Test Standard
Type of extrusion blown - -
注塑熔体温度 180 - 220 °C -
典型数据
加工方法
吹塑挤出成型, 薄膜挤出成型
供货形式
粒料
特征
共聚物, 丁烯共聚物
耐化学试剂
耐酸性, 抗氧化性
Certifications
可食品接触的, 1935/2004/EC认证, 10/2011认证, FDA 21 CFR认证, RoHS
应用
电子电气, 药物, 包装
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.