Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MX731 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MX731:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan™ Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan™ Copolyester MX731 is a high flow medical grade of Eastman Tritan™ that has viscosity reductions of 40-50% relative to Eastman Tritan™ Copolyester MX711. Eastman Tritan™ Copolyester MX731 contains a mold release derived from vegetable based sources. Eastman Tritan™ Copolyester MX731 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt

flowability. Eastman Tritan™ Copolyester MX731 has been formulated for medical devices. Eastman Tritan™ Copolyester MX731 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and ETO sterilization.




加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 1600 MPa ISO 527
屈服应力 44 MPa ISO 527
屈服伸长率 7 % ISO 527
断裂应力 49 MPa ISO 527
断裂伸长率 154 % ISO 527
弯曲模量, 23°C 1500 MPa ISO 178
弯曲强度 60 MPa ISO 178
悬臂梁缺口冲击强度, +23°C 83 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 11 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -40 °C -
ASTM数据
拉伸模量 1575 MPa ASTM D 638
屈服应力 43 MPa ASTM D 638
断裂拉伸强度 52 MPa ASTM D 638
屈服伸长率 7 % ASTM D 638
断裂伸长率 210 % ASTM D 638
弯曲模量 1575 MPa ASTM D 790
洛克硬度 R 111 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 860 J/m ASTM D 256
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 81 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 1 % ASTM D 1003
光透射率 91 % ASTM D 1003
其它性能价值单位Test Standard
密度 1180 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 88 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 260 - 282 °C -
模具温度 38 - 66 °C -
典型数据
加工方法
注塑
添加剂
脱模助剂
特殊性能
经热稳处理的/耐热的, 透明., 消毒, 环氧乙烷灭菌(EtO), Gamma irradiation sterilization
特征
无定形, 颜色稳定性, 共聚物
耐化学试剂
通用耐化学性, 水解稳定, 抗辐射性
Certifications
可食品接触的, FDA 21 CFR认证, 医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.