Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ TX2001 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ TX2001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents Tritan TX2001 copolyester may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan TX2001 is certified to NSF/ANSI Standard 51 for Food Equipment

Materials and is also certified to NSF/ANSI Standard 61 – Drinking Water System Components-Health Effects.




加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 1620 MPa ISO 527
屈服应力 45 MPa ISO 527
屈服伸长率 7 % ISO 527
断裂应力 49 MPa ISO 527
断裂伸长率 130 % ISO 527
弯曲模量, 23°C 1530 MPa ISO 178
悬臂梁缺口冲击强度, +23°C 66 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 14 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -40 °C -
ASTM数据
拉伸模量 1585 MPa ASTM D 638
屈服应力 44 MPa ASTM D 638
断裂拉伸强度 53 MPa ASTM D 638
屈服伸长率 7 % ASTM D 638
断裂伸长率 140 % ASTM D 638
弯曲模量 1585 MPa ASTM D 790
洛克硬度 R 115 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 650 J/m ASTM D 256
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 109 °C ASTM D 648
DTUL @ 264 psi 92 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 1 % ASTM D 1003
光透射率 92 % ASTM D 1003
其它性能价值单位Test Standard
密度 1170 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 88 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 260 - 282 °C -
模具温度 38 - 66 °C -
典型数据
加工方法
注塑
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的, 透明.
特征
无定形, 共聚物
耐化学试剂
通用耐化学性, 水解稳定
Certifications
可食品接触的, FDA 21 CFR认证, NSF 51认证, 可水接触的, NSF认证 61
应用
汽车, 电子电气, 包装, 运动器械, 玩具
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.