Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4300 G2 - PBT-GF10 - BASF

Material Data Center offers the following functions for Ultradur® B 4300 G2:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
具有10 %玻璃纤维的易流动注塑等级, 用于坚硬、 有韧
性、 尺寸稳定的技术零部件 (例如计时控制圆盘、 触发器、 门旋钮、 自动调温器零部件、 烤箱门把手、 烤面包机外壳和烤架)。
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 16 cm³/10min ISO 1133
温度 250 °C -
载荷 2.16 kg -
模塑收缩率, 平行 1.2 % ISO 294-4, 2577
模塑收缩率, 垂直 1.4 % ISO 294-4, 2577
熔体密度 1130 kg/m³ -
熔体 0.18 W/(m K) -
熔体的比热 1990 J/(kg K) -
喷射温度 170 °C -
ASTM数据
模压收缩率, 平行 0.008 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 4400 MPa ISO 527
断裂应力 80 MPa ISO 527
断裂伸长率 4.5 % ISO 527
无缺口简支梁冲击强度, +23°C 37 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 38 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 3.5 kJ/m² ISO 179/1eA
ASTM数据
拉伸模量 4482 MPa ASTM D 638
断裂拉伸强度 90.3 MPa ASTM D 638
断裂伸长率 3.5 % ASTM D 638
弯曲模量 3930 MPa ASTM D 790
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 223 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 165 °C ISO 75-1/-2
热变形温度, 0.45 MPa 210 °C ISO 75-1/-2
线性热膨胀系数, 平行 60 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 125 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
燃烧性-氧指数 19.5 % ISO 4589-1/-2
ASTM数据
DTUL @ 66 psi 220 °C ASTM D 648
DTUL @ 264 psi 200 °C ASTM D 648
熔点 223 °C ASTM D 3418
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.6 - IEC 62631-2-1
相对介电常数., 1MHz 3.6 - IEC 62631-2-1
介质损耗因子, 100Hz 12 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 150 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
介电强度 37 kV/mm IEC 60243-1
相对漏电起痕指数 300 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.4 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1370 kg/m³ ISO 1183
密度 1370 kg/m³ ASTM D 792
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数 115 cm³/g ISO 307, 1157, 1628
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 260 °C ISO 294
注塑, 模具温度 80 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 120 °C -
预干燥-时间 4 h -
加工湿度 ≤0.04 % -
注塑熔体温度 250 - 275 °C -
模具温度 60 - 100 °C -
函数
粘度-剪切速度 , Ultradur® B 4300 G2, PBT-GF10, BASF
剪切应力-剪切速度 , Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变.  , Ultradur® B 4300 G2, PBT-GF10, BASF
正割模量-应变.  , Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变(等时的) 23°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变模量-时间. 23°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变曲线 23°C, Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变(等时的) 40°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变模量-时间. 40°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变曲线 40°C, Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变(等时的) 90°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变模量-时间. 90°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变曲线 90°C, Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变(等时的) 120°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变模量-时间. 120°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变曲线 120°C, Ultradur® B 4300 G2, PBT-GF10, BASF
应力-应变(等时的) 160°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变模量-时间. 160°C, Ultradur® B 4300 G2, PBT-GF10, BASF
蠕变曲线 160°C, Ultradur® B 4300 G2, PBT-GF10, BASF
比容-温度(pvT) , Ultradur® B 4300 G2, PBT-GF10, BASF
拉伸模量-温度 , Ultradur® B 4300 G2, PBT-GF10, BASF
典型数据
加工方法
注塑
供货形式
粒料, 自然色
添加剂
润滑剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
耐化学性
酸类
醋酸 (5g/100g) (23°C)
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.