Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PA - PA666 - BASF

Material Data Center offers the following functions for Ultrafuse PA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 49.5 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 5 / * kg -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 196 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 49 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 65 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 135 / * °C ISO 75-1/-2
维卡软化温度, B 172 / * °C ISO 306
其它性能干 / 已调节单位Test Standard
密度 1110 / 1050 kg/m³ ISO 1183
3D Data干 / 已调节单位Test Standard
Other Standards[S]
拉伸模量, flat 2420 / 395 MPa ISO 527
拉伸模量, upright 2120 / 334 MPa ISO 527
拉伸强度, flat 61.4 / 33.2 MPa ISO 527
拉伸强度, upright 16.4 / 17.6 MPa ISO 527
断裂伸长率, flat 9.6 / 143 % ISO 527
断裂伸长率, upright 0.8 / 12.8 % ISO 527
弯曲模量, flat 2050 / 445 MPa ISO 178
弯曲模量, on-edge 2250 / 468 MPa ISO 178
弯曲模量, upright 2150 / 428 MPa ISO 178
弯曲强度, flat 77 / 17.7 MPa ISO 178
弯曲强度, on-edge 95.5 / 18.1 MPa ISO 178
弯曲强度, upright 40.2 / 17.3 MPa ISO 178
无缺口简支梁冲击强度, +23°C, flat 23 / 0 kJ/m² ISO 179/1eU
无缺口简支梁冲击强度, +23°C, on-edge 29.7 / 0 kJ/m² ISO 179/1eU
无缺口简支梁冲击强度, +23°C, upright 3.5 / 13.4 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, flat 5.6 / - kJ/m² ISO 179/1eA
简支梁缺口冲击强度, +23°C, on-edge 3.3 / 136 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, +23°C, upright 1.2 / 9.4 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C, flat 28 / 0 kJ/m² ISO 180/1U
Izod冲击强度, +23°C, on-edge 45.6 / 0 kJ/m² ISO 180/1U
Izod冲击强度, +23°C, upright 3.2 / 17.4 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, flat 5.8 / 85.4 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, +23°C, on-edge 3.9 / 106 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, +23°C, upright 1.7 / 10.1 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
典型数据
加工方法
Additive Manufacturing
供货形式
单纤纺丝
特征
热稳定性
地区供应
北美, 欧洲, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.