Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse TPU 80A LF - TPU - BASF

Material Data Center offers the following functions for Ultrafuse TPU 80A LF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 82.5 cm³/10min ISO 1133
温度 210 °C -
载荷 10 kg -
机械性能价值单位Test Standard
ISO数据
70°C时恒定应变下的永久变形, 24h 52 % ISO 815
耐磨性 56 mm³ ISO 4649
肖氏硬度A 89 - ISO 7619-1
肖氏硬度D 35 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min -44 °C ISO 11357-1/-2
其它性能价值单位Test Standard
密度 1100 kg/m³ ISO 1183
3D Data价值单位Test Standard
Other Standards[S]
断裂应力, flat 35 MPa ISO 527
断裂应力, upright 7 MPa ISO 527
断裂伸长率, flat 610 % ISO 527
断裂伸长率, upright 230 % ISO 527
简支梁冲击强度, -30°C, flat 0 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C, on-edge 0 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C, upright 0 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, flat 0 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, +23°C, on-edge 0 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, +23°C, upright 0 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C, flat 0 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C, on-edge 0 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C, upright 0 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C, flat 0 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, +23°C, on-edge 0 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, +23°C, upright 0 kJ/m² ISO 180/1A
50%应变时的应力, flat 5.8 MPa ISO 527
50%应变时的应力, upright 4.6 MPa ISO 527
100%应变时的应力, flat 6.9 MPa ISO 527
100%应变时的应力, upright 5.4 MPa ISO 527
200%应变时的应力, flat 11.5 MPa ISO 527
体积电阻率, flat 2.3E10 Ohm*m IEC 62631-3-1
体积电阻率, on-edge 1.6E10 Ohm*m IEC 62631-3-1
体积电阻率, upright 1.6E10 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
典型数据
加工方法
Additive Manufacturing
供货形式
单纤纺丝
地区供应
北美, 欧洲, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com