Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Utec® 5541 - (PE-UHMW) - Braskem

Material Data Center offers the following functions for Utec® 5541:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Utec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体 0.4 W/(m K) -
机械性能价值单位Test Standard
ISO数据
屈服应力 17 MPa ISO 527
断裂应力 30 MPa ISO 527
断裂伸长率 350 % ISO 527
简支梁冲击强度, +23°C 90 kJ/m² ISO 179/1eU
肖氏硬度D 64 - ISO 7619-1
ASTM数据
屈服应力 17 MPa ASTM D 638
断裂拉伸强度 30 MPa ASTM D 638
断裂伸长率 300 % ASTM D 638
邵氏硬度D 64 - ASTM D 2240
悬臂梁缺口冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
维卡软化温度, A 128 °C ISO 306
ASTM数据
热释放速率, 平行 150 E-6/K ASTM D 696
DTUL @ 66 psi 79 °C ASTM D 648
DTUL @ 264 psi 48 °C ASTM D 648
熔点 133 °C ASTM D 3418
维卡温度 128 °C ASTM D 1525
热导率, 固态 0.0577 W/(m K) ASTM C 177
电性能价值单位Test Standard
ASTM数据
电介质强度, 短时 90 kV/mm ASTM D 149
表面电阻率 1E12 Ohm ASTM D 257
体积电阻率 1E14 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水率, 24小时 0.01 % ASTM D 570
密度 925 kg/m³ ASTM D 792
Intrinsic Viscosity 24 dl/g -
Bulk Density 450 kg/m³ -
典型数据
加工方法
其它挤出成型, 模压成型
特殊性能
高冲击韧性的/经抗冲改性的
特征
Tribologic Grade
地区供应
北美, 欧洲, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.