Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 CF30 - PEEK-CF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 CF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Carbon fiber-reinforced (30%), high viscosity polyether ether ketone

VESTAKEEP® 4000 CF30 is a carbon fiber reinforced (30%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CF30 are of low flammability.

VESTAKEEP® 4000 CF30 can be processed by common injection molding machines for thermoplastics.

We recommend a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 CF30 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing VESTAKEEP® 4000 CF30, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines.“

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT WWW.INDUSTRIAL.VESTAKEEP.COM
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 20 cm³/10min ISO 1133
温度 380 °C -
载荷 21.6 kg -
模塑收缩率, 平行 0 % ISO 294-4, 2577
模塑收缩率, 垂直 0.4 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 23000 MPa ISO 527
断裂应力 240 MPa ISO 527
断裂伸长率 2 % ISO 527
无缺口简支梁冲击强度, +23°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
简支梁冲击强度, -30°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
简支梁缺口冲击强度, +23°C 10 kJ/m² ISO 179/1eA
Type of failure C - -
简支梁缺口冲击强度, -30°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 340 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 325 °C ISO 75-1/-2
热变形温度, 0.45 MPa 335 °C ISO 75-1/-2
维卡软化温度, B 340 °C ISO 306
线性热膨胀系数, 平行 10 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
燃烧性-氧指数 47 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 1MHz 17 - IEC 62631-2-1
介质损耗因子, 1MHz 230 E-4 IEC 62631-2-1
体积电阻率 10000 Ohm*m IEC 62631-3-1
表面电阻率 1000000 Ohm IEC 62631-3-2
其它性能价值单位Test Standard
吸水性 0.4 % 类似ISO 62
密度 1400 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 420 °C ISO 294
注塑, 模具温度 200 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
注塑, 保压压力 120 MPa ISO 294
函数
拉伸模量-温度 , VESTAKEEP® 4000 CF30, PEEK-CF30, Evonik
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.