Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M40 3DF - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M40 3DF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Filament based on high viscosity, unreinforced polyether ether ketone (PEEK) for 3D printed medical devices

VESTAKEEP® Care M40 3DF is extruded from naturally colored, high viscosity VESTAKEEP® Care M40 G PEEK resin. The material is designed for 3d printing of medical devices with up to 30 days body contact.  


Biocompatibility

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests available for VESTAKEEP® Care M40 3DF:


Delivery and packaging
VESTAKEEP® Care M40 3DF filament has a diameter of 1.75 mm ( /- 0.04 mm*). It is supplied on TROGAMID®-spools with 500g. The spools are packaged in double bags to facilitate transfer into clean areas.

The properties listed are for information only and only apply to the VESTAKEEP® Care M40 G resin used in the manufacture of VESTAKEEP® Care M40 3DF. The performance and the purity of any parts manufactured from VESTAKEEP® Care M40 3DF are highly dependent on any 3D- or additive-printing processes, or any other processing, to which the filament is subjected.
Only density and filament diameter apply to VESTAKEEP® Care M40 3DF directly.

*Diameters are tested by a multi-axis laser gauge. The diameter is the average of these axis.


The values presented are typical or average values, they do not constitute a specification. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 11 cm³/10min ISO 1133
温度 380 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 3500 MPa ISO 527
拉伸强度 94 MPa ISO 527
屈服应力 94 MPa ISO 527
屈服伸长率 5 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 7 kJ/m² ISO 179/1eA
Type of failure C - -
简支梁缺口冲击强度, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 335 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 152 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 155 °C ISO 75-1/-2
热变形温度, 0.45 MPa 205 °C ISO 75-1/-2
维卡软化温度, A 335 °C ISO 306
维卡软化温度, B 305 °C ISO 306
线性热膨胀系数, 平行 60 E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 3.2 mm -
ASTM数据
熔点 335 °C ASTM D 3418
其它性能价值单位Test Standard
吸水性 0.4 % 类似ISO 62
密度 1300 kg/m³ ISO 1183
密度 1300 kg/m³ ASTM D 792
典型数据
加工方法
Additive Manufacturing
供货形式
单纤纺丝, 自然色
特殊性能
经热稳处理的/耐热的, Opaque
特征
热稳定性
耐化学试剂
耐酸性, 耐碱性, 通用耐化学性, 耐溶剂性, 耐油脂性, 水解稳定, 耐油性, 抗氧化性
Certifications
医用级, US药物六级认证
应用
药物
地区供应
欧洲
其他信息
其E烦龀尚
Drying recommendations 干燥建议

We recommend to dry the filament prior to usage to avoid stringing, bubbles, or other defects. 
建议长丝在使用前进行干燥以避免拉丝、气泡或其它缺陷的产生

a) Filament on spool: minimum 12 hours at 80°C to 100°C. 100°C must not be exceeded to avoid distortion of the spool.
  • 丝盘上的长丝:80°C- 100°C,不能低于12小时。禁止超过100°C以避免丝盘变形。

b) Filament removed from spool: minimum 4 hours at 130°C to 140°C.
  • 不带丝盘的长丝:130°C - 140°C,不能低于4小时。


The maximum drying temperature of the filament is 140°C. Please also pay attention to the instructions of your drying device.
长丝的干燥温度不能超过140°C。请注意干燥设备的使用说明。



Spool dimensions 丝盘尺寸

For dimensions of the spool, please see drawing below. All dimensions are given in millimeter (mm).
丝盘尺寸见下图。尺寸单位均为毫米(mm)
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.