Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS2211 BK E70405 - PA610... - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS2211 BK E70405:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid Terra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
High-viscosity, heat- and light-stabilized Polyamide 610 Compound for extrusion
VESTAMID® Terra HS2211 BK E70405 is a polyamide 610 compound developed for the manufacturing of tubing systems with higher demands on heat resistance.

The melting range of VESTAMID® Terra HS2211 BK E70405 is about 40°C higher than PA 11 and PA 12 compounds and allows higher peak temperatures in use.

The compound is especially suitable for the extrusion of tubing systems that are exposed to high burst pressures at high service temperatures, e.g., hydraulic clutch lines. The process temperatures should be within a range of 240°C to 270°C.

VESTAMID® Terra HS2211 is delivered as cylindrical granules ready for processing in moisture-proof packaging. 

VESTAMID® Terra HS is partly based on renewable raw materials and fills the performance gap between the commodity and the niche long-chain nylons.
VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources
.

Pigmentation may affect values.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 19 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 5 / * kg -
模塑收缩率, 平行 1.6 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.3 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 2500 / - MPa ISO 527
屈服应力 66 / - MPa ISO 527
屈服伸长率 4 / - % ISO 527
名义断裂伸长率 >50 / - % ISO 527
无缺口简支梁冲击强度, +23°C N / - kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
简支梁缺口冲击强度, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 222 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 42 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 54 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 155 / * °C ISO 75-1/-2
维卡软化温度, B 195 / * °C ISO 306
线性热膨胀系数, 平行 95 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 94 / * E-6/K ISO 11359-1/-2
其它性能干 / 已调节单位Test Standard
吸水性 3.5 / * % 类似ISO 62
吸湿性 1.7 / * % 类似ISO 62
密度 1060 / - kg/m³ ISO 1183
典型数据
加工方法
管材挤出, 其它挤出成型
供货形式
粒料, 碎粒料, 黑色
添加剂
脱模助剂
特殊性能
经光稳处理的/耐光的, 经热稳处理的/耐热的
Certifications
生物相容
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.