Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9325 BK E70352 - PA612-GF40 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9325 BK E70352:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Heat-stabilized, glass fiber-reinforced, PA 612 compound for plastic-EPDM-rubber bonds

VESTAMID® DX9325 BK E70352 is a glass fiber-reinforced, PA 612 molding compound. The material contains about 40% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9325 BK E70352 is especially suitable for the production of plastic and rubber composites. 

Parts of VESTAMID® DX9325 BK E70352 can be co-vulcanized with EPDM-rubbers without using any adhesives or adhesion promoters ("direct-bonding to rubber"). Because of its semi-crystalline morphology VESTAMID® DX9325 BK E70352 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids.

VESTAMID® DX9325 BK E70352 is supplied as cylindrical pellets ready for processing in moisture-proof bags.

Very important are predrying conditions. The material has to be handle as plasticized PA 612. The drying temperature should be not more than 80°C and the drying time at this temperature not more than 4h.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 0.2 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.7 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 10300 / - MPa ISO 527
断裂应力 160 / - MPa ISO 527
断裂伸长率 4.4 / - % ISO 527
无缺口简支梁冲击强度, +23°C 100 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
简支梁冲击强度, -30°C 104 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
简支梁缺口冲击强度, +23°C 18 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
简支梁缺口冲击强度, -30°C 16 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
热性能干 / 已调节单位Test Standard
ISO数据
热变形温度, 1.80 MPa 200 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 215 / * °C ISO 75-1/-2
其它性能干 / 已调节单位Test Standard
密度 1410 / - kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
粒料, 黑色
添加剂
脱模助剂
特殊性能
经光稳处理的/耐光的, 经热稳处理的/耐热的
特征
好粘附性能
耐化学试剂
通用耐化学性, 耐油脂性, 耐油性
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.