Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9041 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9041 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Medium-viscosity, heat and light stabilized polyamide 12 compound

VESTAMID® LX9041 BK 9.7504 s a heat stabilized and light resistant polyamide 12 compound especially developed for extrusion coating of steel tubes.
 
Due to the exceptional impact strength, abrasion resistance and good chemical resistance of PA 12 as well as the excellent adhesion between the steel and the properly applied VESTAMID® LX9041 BK 9.7504 , the corrosion resistance of steel tubes coated with VESTAMID® LX9041 black is significantly increased.

VESTAMID® LX9041 BK 9.7504 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 17 / * cm³/10min ISO 1133
温度 240 / * °C -
载荷 2.16 / * kg -
模塑收缩率, 平行 1.1 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.1 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1730 / 1370 MPa ISO 527
屈服应力 51 / 44 MPa ISO 527
屈服伸长率 4 / 12 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
无缺口简支梁冲击强度, +23°C N / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 4 / 3.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
简支梁缺口冲击强度, -30°C 4.3 / 4 kJ/m² ISO 179/1eA
Type of failure C / C - -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 177 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 44 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 48 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 120 / * °C ISO 75-1/-2
维卡软化温度, B 141 / * °C ISO 306
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 3.7 / 4.4 - IEC 62631-2-1
相对介电常数., 1MHz 3.1 / 3.2 - IEC 62631-2-1
介质损耗因子, 100Hz 330 / 610 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 195 / 363 E-4 IEC 62631-2-1
体积电阻率 9.3E12 / 4.9E12 Ohm*m IEC 62631-3-1
其它性能干 / 已调节单位Test Standard
吸水性 1.3 / * % 类似ISO 62
吸湿性 0.7 / * % 类似ISO 62
密度 1020 / - kg/m³ ISO 1183
典型数据
加工方法
表面涂层
供货形式
粒料, 黑色
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经热稳处理的/耐热的
特征
好粘附性能
耐化学试剂
通用耐化学性
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com