Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ME47 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ME47:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Polyamide 12 elastomer molding compounds

VESTAMID® Care ME47 is free of plasticizers and heat and light stabilized. VESTAMID® Care ME47 is resistant to body fluids and toxicologically safe.

VESTAMID® Care ME grades are flexible polyether block amides (PEBA) resins.

The advantages at a glance:
  • High flexibility & elasticity
  • Good rebound properties
  • High impact resistance
  • Excellent dimensional stability
  • High chemical resistance
  • Easy processability & colorability
  • Plasticizer-free
  • Gamma and EtO sterilization resistant
  • Tough and resilient

Biocompatibility of VESTAMID® Care ME

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation


Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 28 / * cm³/10min ISO 1133
温度 240 / * °C -
载荷 2.16 / * kg -
模塑收缩率, 平行 0.3 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.8 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 125 / - MPa ISO 527
拉伸蠕变模量, 1000h * / 90 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N / - kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C N / - kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C N / - kJ/m² ISO 179/1eA
肖氏硬度D 47 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 157 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -50 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 45 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 65 / * °C ISO 75-1/-2
维卡软化温度, B 70 / * °C ISO 306
线性热膨胀系数, 平行 230 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 210 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 8.5 / - - IEC 62631-2-1
相对介电常数., 1MHz 4.7 / - - IEC 62631-2-1
介质损耗因子, 100Hz 1200 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 1300 / - E-4 IEC 62631-2-1
体积电阻率 1E9 / - Ohm*m IEC 62631-3-1
其它性能干 / 已调节单位Test Standard
吸水性 1 / * % 类似ISO 62
吸湿性 0.4 / * % 类似ISO 62
密度 1020 / - kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 200 °C ISO 294
注塑, 模具温度 35 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经热稳处理的/耐热的, 消毒, 环氧乙烷灭菌(EtO), Gamma irradiation sterilization
耐化学试剂
通用耐化学性
Certifications
医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.