Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L2170 OR E20005 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L2170 OR E20005:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
High viscosity, heat- and light-stabilized polyamide 12 resin

VESTAMID® L2170 OR E20005 has been designed especially for the extrusion of cable sheathings, but it can be used advantageously also for the manufacture of semi-finished products like tubes, rods, sheets and profiles.
 
As a partially crystalline Polyamide 12, VESTAMID® L2170 OR E20005 exhibits a low coefficient of friction which eases the installation of cables in ducts. Sheathings made of VESTAMID® L2170 OR E20005 protect direct buried cables from attack by termites and rodents, due to their tough and smooth surface finish.

Because of low water absorption parts produced from VESTAMID® L2170 OR E20005 maintain their dimension in environments with varying humidity levels, while maintaining a high toughness, a low coefficient of friction and good chemical resistance.
 
VESTAMID® L2170 OR E20005 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
Pigmentation may affect values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30 °C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 3.4 / * cm³/10min ISO 1133
温度 230 / * °C -
载荷 2.16 / * kg -
模塑收缩率, 平行 0.7 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.3 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1650 / - MPa ISO 527
屈服应力 46 / - MPa ISO 527
屈服伸长率 4 / - % ISO 527
名义断裂伸长率 >50 / - % ISO 527
无缺口简支梁冲击强度, +23°C N / - kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
简支梁缺口冲击强度, -30°C 7 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
肖氏硬度D 72 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 178 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 44 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 50 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 110 / * °C ISO 75-1/-2
维卡软化温度, B 148 / * °C ISO 306
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.5 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 3.0 / * mm -
Yellow Card 现存 是的 / * - -
燃烧性-氧指数 24 / * % ISO 4589-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 4.1 / - - IEC 62631-2-1
相对介电常数., 1MHz 3 / - - IEC 62631-2-1
介质损耗因子, 100Hz 700 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 353 / - E-4 IEC 62631-2-1
体积电阻率 9.2E12 / - Ohm*m IEC 62631-3-1
相对漏电起痕指数 600 / - - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.6 / * % 类似ISO 62
吸湿性 0.8 / * % 类似ISO 62
密度 1020 / - kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 240 °C ISO 294
注塑, 模具温度 60 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
典型数据
加工方法
注塑, 管材挤出, 异型材挤出成型, 片材挤出成型, 电线挤出
供货形式
粒料
特殊性能
经光稳处理的/耐光的, 经热稳处理的/耐热的
特征
Tribologic Grade
耐化学试剂
通用耐化学性
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.