Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of XAREC® SP 151 - (PS-SY)-GX30 - Idemitsu Chemicals

Material Data Center offers the following functions for XAREC® SP 151:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
机械性能价值单位Test Standard
ISO数据
拉伸模量 11000 MPa ISO 527
断裂应力 100 MPa ISO 527
断裂伸长率 2.1 % ISO 527
弯曲模量, 23°C 9800 MPa ISO 178
简支梁冲击强度, +23°C 32 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 9 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C 29 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C 10 kJ/m² ISO 180/1A
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 190 °C ISO 75-1/-2
热变形温度, 0.45 MPa 265 °C ISO 75-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
电性能价值单位Test Standard
ISO数据
相对介电常数, 1MHz 3.4 - IEC 62631-2-1
介质损耗因子, 1MHz 10 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
相对漏电起痕指数 600 - IEC 60112
ASTM数据
电介质强度, 短时 50 kV/mm ASTM D 149
耐电弧性 90 s ASTM D 495
其它性能价值单位Test Standard
密度 1410 kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
可电镀的, 高冲击韧性的/经抗冲改性的
应用
汽车, 电子电气
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.