Material datasheets available free. Online registration at: www.materialdatacenter.com
Baypren - CR - LANXESS Deutschland GmbH
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Baypren" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...d by a patented terpolymerisation process with a third monomer. Despite the virtual stagnation in the consumption of halogenated hydrocarbons, some specialties are a talking point: a robust rubber hose made from the Lanxess CR Baypren inflates radially under high internal pressure (Fig.6). Since it contracts at the same time, it acts as an artificial muscle that can safely move even high loads with many times the tensile force of pneumatic pistons. The good aging behaviour of chloroprene rubber...
Kunststoffe international, 2008-01-15, Elastomer Industry Has Understood
... Key features of high-quality models include excellent insulation, lightweight design, good abrasion resistance, and a natural, comfortable feel. That is why manufacturers choose special-purpose Baypren rubber from Lanxess for many types of wetsuits (Fig.10). Sulfurous rubbers are particularly suitable for use on and below the water as their strengths include a combination of excellent thermal insulation properties, good tensile strength and good ozone resistance. The Baypren "sulfur grades&...
Kunststoffe international, 2010-04-20, From Natural Rubber to High-Tech Material
...s aging behavior. Synthetic rubbers are used for flame retardant cable sheathing, weathering resistant seals and even UV stable translucent rubber articles (Fig. 4). Air springs made from dynamically loadable variants such as Baypren (polychloroprene rubber, CR) can survive millions of working cycles without fatigue and are not sensitive to oxygen or ozone (Fig. 5). Hand in hand with the new rubbers an increasingly sophisticated application technology developed: Without detailed know-how, for in...
Kunststoffe international, 2013-08-19, Focus on “Green” Mobility
...ve NBR grades and new Baymod powder NBR grades. An innovative compounding step in polychloroprene production extends the range of applications for this rubber. “With the help of this step, we now have two new product families, Baypren HP and GF, in the pipeline. Baypren HP includes products with properties that are not yet available on the market,” said Jan Paul de Vries, head of High Performance Elastomers. Among the polyethylene-vinyl acetate (EVM) Levapren materials under development, a grade...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.