Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Borsoft" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... PPR 3221 is suitable for transparent bottles produced by blow moulding; it can be processed over a broad range of temperatures and is noted for its exceptional transparency and surface gloss, even if extruded at low temperatures. Borclear and Borsoft are new PP grades from Borealis, which now permit PP blown films to compete with PE products (Fig.2). These grades are transparent and superior to PE in terms of their tactile properties and mechanical strength. Exxon's PP5122E1 is a PP for f...
Kunststoffe international, 2005-11-21, Innovations Today and Tomorrow: Polypropylene for Flexible Packaging
...ciality plastics. Fig. 3 shows the main relationships between the optical properties and the stiffness characteristics of the most important new PP developments. One very special development is that of the flexible random-heterophasic Borsoft grades with their relatively good transparency. They have led to a breakthrough in the production of transparent bags for liquids, and have proved to be an effective substitute for glass bottles and PVC bags in medical packaging (Fig. 4). In contrast, the ...
Kunststoffe international, 2005-11-21, Polypropylene (PP)
...ratures (hot-fill applications) and an improved water vapour barrier (+15%) being just a logical extension of previous trends. Even more interestingly, soft, ductile and transparent random block-copolymers (e.g. Borsoft from Borealis) are based on the same morphology design concepts as mentioned above in the case of Borpact injection moulding grades (see Fig.5). Borsoft copolymers are mainly used in co-extrusion and blends for food, medical and technical films. A very strong application trend f...
Kunststoffe international, 2005-11-21, Polypropylene Films: Versatile Packaging Solutions
...barrier properties and also in printability (Fig.4). For flexible films used in the medical sector – e.g. for infusion bags (title picture) – PP is become established as an important alternative to plasticised PVC (PVC-P). A good example is Borsoft SD233CF, which is used primarily for cast films and, if required, can also be used in special compounds with external elastomers and in coextruded constructions. This material also has special advantages in sterilisation. The sterilisation behaviour ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.