Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Cellophane - CH - Innovia Films Ltd

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Cellophane" in Material Data Center leads to the following information:

Tradename: Cellophane
Family: CH
Producer: Innovia Films Ltd
10 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Back to Nature
...sparent dishes for fresh products – fruit, pasta and delicacies – are available in different sizes. Added to which, there is cling film and film overlay for hot-seal applications. Like cellophane, which also comes in degradable variants, PLA has a high twisting strength for twist-off packaging, which is of central importance for the confectionery industry. Vertical and horizontal flow-pack packaging is completely new. Deep-freeze packaging film has come to the front of the development pipeline a...

Kunststoffe international, 2005-11-21, Innovations Today and Tomorrow: Polypropylene for Flexible Packaging
...nce, and good optical properties and punching characteristics. This has opened up a wide range of new applications. Typical examples are special films for labels (Fig. 5), food packs for cheese, snacks and cake, and the substitution of cellophane in the twist-film segment for sweet, pill and confectionery packs. Finally, the development of the new Borclear C3/C4 polymers, copolymers and terpolymers has resulted in a well-balanced combination of properties, ranging from excellent optical charact...

Kunststoffe international, 2005-11-21, New Material with Potential: Cycloolefin Copolymer (COC)
...truded blown or flat film can be produced. The approximately 30µm thick film possesses excellent optical quality, rugged processability on standard packaging machinery and considerable cost benefits versus the still widely encountered cellophane. COC twist films are already being employed today around the world. The costs of cycloolefins are very dependent on the particular specifications profile. Considerably more effort and expense are required for the medical and optical segments, where the h...

Kunststoffe international, 2005-11-21, Statistical Pitfalls: Packaging - The Plastic Industry's Largest Customer
...emist Jacques Edmund Brandenberger, who worked on developing viscose in a French textile factory, hit upon the idea of coating tablecloths with a solution of viscose. Although he was unsuccessful, a patent was subsequently filed for the invention of cellophane in the year 1908. Ever since, plastic packaging has been an accepted component of our commodities world. However, it was not until industrial production started in the 1950s that it became a major player among packaging materials. In the y...

Kunststoffe international, 2005-11-21, Trends in Laminating Adhesives
...ature stability, barrier properties, mechanical strength and decorative appeal. The range of plastic films and metal foils used for such laminates extends from polyethylene, polypropylene and paper to rigid PVC, polyvinylidene fluoride, polyimide, cellophane, polyester, polyamide, tin, lead and aluminium. The plastic films are often metallized with aluminium or coated with PVDC or SiOx to improve the barrier properties or the light stabilization. Solvent-based Laminating Adhesives At that time...

Kunststoffe international, 2006-09-05, MDO Technology: Defined Stretching
...perties. The main properties concerned are strength, elastic modulus, ultimate elongation, tear strength, stiffness, transparency, gloss, density and barrier properties. This process started to gain large-scale industrial importance in the 1970s, as cellophane and cellulose acetate were replaced with biaxially stretched PP or PET film. Uniaxially stretched flexible film of PP and PE have also long been used as breathable hygienic film, stretch films and tape applications. Optimised Film Propert...

Kunststoffe international, 2012-07-23, Invisible Barrier Features
...flexible plastics packaging – with bi-axially oriented films being used in nearly every application. The successful career of these plastics films started in the mid 1960s when BOPP (bi-axially orientierted polypropylene) increasingly replaced cellophane (Fig. 1). Nowadays BOPP is used for a wide variety of food packaging, as are BOPET, BOPA and BOPS. In different process units the films are metallized, printed, coated and then laminated to create a packaging compound. Such flexible packaging is...

Kunststoffe international, 2012-11-26, Both Ecological and Economical
... permeation and their water vapor barrier needs to be significantly improved through the surface functionalization (Fig 1). The Gerbier HDS SCC (Sized, Coated, Calandered) paper from Ahlstrom Oyj, Helsinki, Finland, and NatureFlex NP cellophane from Innovia Films Ltd., Wigton, Great Britain were used as substrates. These substrates were each coated with different Mowiol polyvinyl alcohol types (PVOH:partly saponified to fully saponified) from Kuraray Europe GmbH, Hattersheim am Main, Germany, on...

Kunststoffe international, 2013-02-22, Is the Future of Plastics “Green”?
... by crosslinking with formaldehyde. The name is derived from the Greek words gala (milk) and lithos (stone). Prominent examples of biobased polymers include modified celluloses such as nitrocellulose (celluloid and parkesine), regenerated cellulose (cellophane), and cellulose acetate, as well as Chitosan produced from chitin. Vegetable fibers and wood flour are used in numerous thermoplastic and thermosetting compounds (wood-plastic compounds, WPC). Even today, natural rubber still accounts for ...

Kunststoffe international, 2014-08-19, New Ideas and Political Markets
...dable polyesters in combination with starches and PLA dominate this segment. They have been used for multi-layer packaging films for several years. This is happening more and more often in combination with cellophane, since they bring a very good innate oxygen and aroma barrier with them. Quality packaging can be manufactured this way for tee, coffee or muesli. Their relatively high permeability to moisture can be reduced to a low level by a combination of materials or a very thin silicate or al...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.