Material datasheets available free. Online registration at: www.materialdatacenter.com
Cyrolite - MBS, PMMA - Röhm GmbH
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Cyrolite" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
..., material manufacturers such as Evonik focus on developing and modifying thermoplastics to resist attack by specialty chemicals used in healthcare.The specialty molding compounds based on polymethyl methacrylate (PMMA) produced under the brand name Cyrolite are transparent, impact-modified copolymers specially developed for medical technology. They are particularly suitable for use in medical device technology and diagnostics equipment. Cyrolite products are available in eight grades with nuanc...
Kunststoffe international, 2005-11-21, PMMA Successful in More and More Fields of Application: Polymethyl Methacrylate (PMMA)
...omobile manufacture and the demanding requirements for modern lighting concepts. It is these compounds that make many of the technical developments and creative design applications possible in the first place. With the brands Plexiglas, Plexalloy, Cyrolite and XT Polymer, the Methacrylates Business Unit of Degussa AG can offer developers a complete range of standard and specialty compounds for all injection and extrusion applications. Variety of New Applications from Coextrusion Among the appli...
Kunststoffe international, 2005-11-21, Polymethyl Methacrylate (PMMA)
...tics, for example polycarbonate. This is due to its clearly superior weather resistance. Prospects In medical technology, one speciality from the field of methacrylate copolymers is finding increasing application. This is Cyrolite, developed by Degussa. Special grades of this copolymer can be sterilised with gamma rays and supplement the range. Interesting fields of application for PMMA sheets are also opening up in the leisure, holiday and fitness sector. Degussa has developed new Plexiglas g...
Kunststoffe international, 2014-10-10, Polymethyl Methacrylate (PMMA)
...s can now dive to over 1,000 m while comfortably contained in a sphere 2.1 m in diameter as if they were floating freely in the water. PMMA also repeatedly contributes to new developments in medical technology. With Cyrolite Protect 2, a new PMMA-based microbe resistant compound has now been approved for the European market and can be used for a variety of applications such as disposable medical instruments or infusion accessories. Furthermore, the material may be sterilized, is resistant to fat...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.