Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Daploy" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...s than other HMS-PP grades. It also produces very low densities and good mechanical properties. New Daploy WB260HMS from Borealis A/S of Denmark is available here from Transmit Technology Group, Borea...
Kunststoffe international, Easier to Reach the Destination
...shown that more than one third of battery power is used for air-conditioning. Improved temperature management is thus crucial to achieving greater range. Borealis Daploy high melt strength polypropylene (HMS PP) products are used to replace rigid plastic materials in numerous automotive applications, including roof liners, moisture barriers in door modules, and lightweight air ducts. HMS PP products combine both high melt strength and extensibility in the melt phase. They open up the possibilit...
Kunststoffe international, 2005-11-21, Innovations Today and Tomorrow: Polypropylene for Flexible Packaging
...e high melt viscosity, it is above all the extensibility behaviour of the melt – the strain hardening – that essentially governs the processing properties during coating, foaming and blown film extrusion [8]. Through the use of Daploy HMS (a newly developed HMS-PP), it has now become possible to obtain a combination of melt strength and extensibility comparable with PE-LD. In practical terms, it means that, for the first time, PP can be made to expand much more easily with very low foam densitie...
Kunststoffe international, 2005-11-21, Polymer Design and Modification: Polypropylene (PP)
...it is possible to provide a wide range of properties from rigid and temperature-resistant low-density packaging materials to very soft foams (Fig. 2). The introduction of long-chain branched statistical copolymers with the designation Daploy WB260HMS (Borealis) represents one of the most recent development in this field. While the modulus of elasticity of long-chain branched homopolymers is between 1600 and 2000MPa, and is thus suitable for rigid applications (especially packaging), long-chain ...
Kunststoffe international, 2005-11-21, Polypropylene Films: Versatile Packaging Solutions
...ackaging (MAP) for bread and bakery products (Fig.3) and labels. Further developments with PP blown film can be predicted. Grades with bimodal molecular weight distribution are a possibility, while another is long-chain-branched HMS-PP (grade: Daploy HMS) with high melt strength, which is also significantly extending the range of possible applications for PP in foamed materials, extrusion coating and blow moulding [3]. In this case, advantages are also gained through combination with the nuclea...
Kunststoffe international, 2010-01-27, Value Creation through Innovation
...cts made from this foam can be found in automobiles, insulation, food containers and protective packaging. In Europe polypropylene foam applications are mainly found in the food and automobile sectors. The newly developed product Daploy WB 140HMS, which is based on a long chain branched polypropylene with densities down to 35 kg/m3, is particularly suitable for applications in catering and microwave tableware. It is also envisaged that a newly developed high performance polypropylene should be a...
Kunststoffe international, 2011-10-17, Polypropylene (PP)
...olymer which permits high-speed production of optically perfect polymer films, and is also sterilizable [3]. When PP is processed as blown film, however, the problem of bubble instability becomes more acute with increase in production speed. Daploy WB180HMS from the family of long-chain branched polypropylenes which only Borealis currently offers can be of service here. Add a few percent to the film formulation (preferably to the middle layer) and production can be boosted by up to 40 %. As Dapl...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.