Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Disflamoll" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...0% additive. Selection of suitable flame retardants proved difficult because the relevant commercial suppliers had absolutely no experience with this type of product. The following products were supplied by Lanxess, Leverkusen/Germany: Disflamoll DPK (active ingredient diphenyl cresyl phosphate), Disflamoll TOF (active ingredient trioctyl phosphate), Levagard TEP (active ingredient triethyl phosphate) and Levagard DMPP (active ingredient dimethyl propane phosphonate). In addition, the flame reta...
Kunststoffe international, 2010-09-24, A Motley Range of Innovations
...o complex surfaces. The substrate dries quickly and offers high fire resistance combined with improved thermal insulation performance and additional sound-absorbing properties. PVC synthetic leather will benefit from flame-retardant finishing with Disflamoll TP LXS 51 036, which also makes an ideal plasticizer. Levagaard DMPP is a highly effective flame retardant with a very high phosphorus content. Due to its low viscosity, it is ideal for use in rigid foams, coatings, adhesives, epoxy resins a...
Kunststoffe international, 2012-11-26, Demands and Innovations
...cations that can also be used in combination with phosphates, Uniplex FRX 4494S (an EDAP/melamine blend) for polyolefins and Uniplex FRP-64 (poly-2,6-dibromophenylene oxide), a brominated flame retardant for PBT, PA6 and PA66. The Disflamoll range with the classic phosphate esters includes an interesting new flame retardant, Disflamoll TP LXS 51036, developed specially for imitation leather. In the Levagard range which is particularly suitable for flame retarding polyurethane rigid foams, Levaga...
Kunststoffe international, 2015-09-18, Regulations, Markets, Trends
... halogen-free, flame retardants based inter alia on a newly developed type of phosphorus chemistry. They are characterized by low fogging and low scorching and thus are ideally suited for use in the furniture and automotive industry. Their new Disflamoll TP LXS 51092 was mainly developed for PU flexible foams and elastomers; Levagard TP LXS 51114 (Fig. 2) for flexible foams. Both flame retardants can be used in polyesters as well as in polyether flexible foams. Foams produced with Levagard TP LX...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.