Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Grilamid" in Material Data Center leads to the following information:

Tradename: Grilamid
Family: PA12, TPA
Producer: EMS-GRIVORY | a unit of EMS-CHEMIE AG
167 hits in the material database
20 hits in the literature database
11 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
Grilamid Water mainfold of a shower faucet
Grilamid TR 90 Water filter
Grilamid TR Headphones
Grilamid TR Baby bottle
Grilamid TR Ballpoint pen
Grilamid Heel shell of a touring ski boot
Grilamid LCL-3 H anthracite Neck protection
Grilamid LCL-3 H anthracite Knee brace
Grilamid L 20A HL NZ nat Touring ski boot
Grilamid LCL-3 H anthracite Rear frame, Husqvarna motorcycles
Grilamid TR Housing and cover, hearing aid

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.