Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Grivory - PA6I/6T, PPA - EMS-CHEMIE

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Grivory" in Material Data Center leads to the following information:

Tradename: Grivory
Family: PA6I/6T, PPA
Producer: EMS-CHEMIE
83 hits in the material database
48 hits in the literature database
25 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
Grivory HTV-5H1 nat Plastic screw DELTA PTĀ®
Grivory HT3 Plugs and connectors
Grilamid Water mainfold of a shower faucet
Grivory HT1V FWA Water meter
Grilamid TR 90 Water filter
Grivory HT1V FWA Frying spatula
Grilamid TR Headphones
Grilamid TR Baby bottle
Grilamid TR Ballpoint pen
Grivory GV-5H Bracket for a car windshield washer
Grilamid Heel shell of a touring ski boot
Grilamid LCL-3 H anthracite Neck protection
Grilamid LCL-3 H anthracite Knee brace
Grilon TSGL-50-4 nat Rear seatback, Audi A8
Grilamid L 20A HL NZ nat Touring ski boot
Grivory HT1VL-50X Gear shift module
Grilon TSGL-40/4 nat Exterior mirror holder for trucks
Grivory GVL-4H nat Housing of exterior light TESIS
Grilon TSGL-50-4 nat Stirrup
Grivory HT2VS-3HH Emergency gear release
Grilon TSG-35/4 W2 Resonator
Grilamid LCL-3 H anthracite Rear frame, Husqvarna motorcycles
Grilamid TR Housing and cover, hearing aid
Grivory HT XE 10827 Water outlet brackets
Grivory HT1VA-35 HYS Cooling water valve

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.