Hostalen - PE-HD, PP - LyondellBasell Industries

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Hostalen" in Material Data Center leads to the following information:

Tradename: Hostalen
Family: PE-HD, PP
Producer: LyondellBasell Industries
89 hits in the material database
28 hits in the literature database
2 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Hostalen 4131 B (PE-HD)
Hostalen 4731 B (PE-HD)
Hostalen 5052 B BLACK (PE-HD)
Hostalen ACP 5231 D (PE-HD)
Hostalen ACP 5331 A (PE-HD)
Hostalen ACP 5331 H (PE-HD)
Hostalen ACP 5531 B (PE-HD)
Hostalen ACP 5831 D (PE-HD)
Hostalen ACP 6031 D (PE-HD)
Hostalen ACP 6541A UV (PE-HD)
Hostalen ACP 7740 F2 (PE-HD)
Hostalen ACP 7740 F3 (PE-HD)
Hostalen ACP 9240 Plus (PE-HD)
Hostalen ACP 9255 Plus (PE-HD)
Hostalen CRP 100 BLACK (PE-HD)
Hostalen CRP 100 BLACK (XL) (PE-HD)
Hostalen CRP 100 Orange (PE-HD)
Hostalen CRP 100 RD BLACK (PE-HD)
Hostalen CRP 100 RESIST CR BLACK (PE-HD)
Hostalen CRP 100 RESIST CR orange (PE-HD)
Hostalen CRP 100 RESIST CR W Blue (PE-HD)
Hostalen CRP 100 RESIST S Blue (PE-HD)
Hostalen CRP 100 RESIST S Brown (PE-HD)
Hostalen CRP 100 RESIST S Orange-yellow (PE-HD)
Hostalen CRP 100 RT BLACK (PE-HD)
Hostalen CRP 100 S Blue (PE-HD)
Hostalen CRP 100 S Brown (PE-HD)
Hostalen CRP 100 S Orange-yellow (PE-HD)
Hostalen CRP 100 S RED (PE-HD)
Hostalen CRP 100 S Yellow (PE-HD)
Hostalen CRP 100 W Blue (PE-HD)
Hostalen GC 7258 (PE-HD)
Hostalen GC 7260 (PE-HD)
Hostalen GC 7260 F2 (PE-HD)
Hostalen GC 7260 LS (PE-HD)
Hostalen GD 4755 (PE-HD)
Hostalen GD 7255 (PE-HD)
Hostalen GD 7255 LS (PE-HD)
Hostalen GD 9550 F (PE-HD)
Hostalen GF 4750 (PE-HD)
Hostalen GF 7750 M2 (PE-HD)
Hostalen GF 9045 F (PE-HD)
Hostalen GF 9055 F (PE-HD)
Hostalen GM 5010 T3 BLACK (PE-HD)
Hostalen GM 5010 T3 S Blue (PE-HD)
Hostalen GM 5010 T3 S Brown (PE-HD)
Hostalen GM 5010 T3 S RED (PE-HD)
Hostalen GM 5010 T3 S Yellow (PE-HD)
Hostalen GM 9240 HT (PE-HD)
Hostalen GM 9310 C BLACK (PE-HD)
Hostalen GM 9350 C BLACK (PE-HD)
Hostalen GX 9254 (PE-HD)
Hostalen PP EBG 252D PP-GF10
Hostalen PP EPD60R PP
Hostalen PP H1022 PP
Hostalen PP H1022 12 PP
Hostalen PP H1850 PP
Hostalen PP H2142 12 PP
Hostalen PP H2150 PP
Hostalen PP H2150 304850 PP
Hostalen PP H2150-RC PP
Hostalen PP H2222 36 PP
Hostalen PP H2250 36 PP
Hostalen PP H2450 PP
Hostalen PP H2464 PP
Hostalen PP H2483 PP
Hostalen PP H4122 103220 PP
Hostalen PP H5416 PP
Hostalen PP H7350FLS 303064 PP
Hostalen PP HP1886 PP
Hostalen PP W2080 PP
Hostalen PP XN112-I PP
Hostalen PP XN125-P PP
Hostalen ACP 9254 Plus (PE-HD)
Hostalen QCP 5404 Black (PE-HD)
Hostalen QCP 5603 Ivory Plus (PE-HD)
Hostalen QCP 5404 Ivory (PE-HD)
Hostalen QCP 5603 Grey (PE-HD)
Hostalen QCP 5603 Ivory (PE-HD)
Hostalen QCP 5603 Grey Plus (PE-HD)
Hostalen QCP 5404 Grey (PE-HD)
Hostalen 5231H UV (PE-HD)
Hostalen 5231H (PE-HD)
Hostalen GX5044 (PE-HD)
Hostalen PP H2212 36 PP
Hostalen PP H2493 PP
Hostalen CRP 100 RCD BLACK (PE-HD)
Hostalen GF 7750 M3 (PE-HD)
Hostalen ACP 9255 B (PE-HD)

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.