Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Hytemp" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...content (up to 90 to 95%) in contrast to its competitors with their more plastic rubber types (vinyl acetate content: 40 to 60%). The acrylic rubbers (ACM) HyTemp and Nipol AR (Zeon) have become established in recent years for large-area hot-oil seals (oil sump, engine hood, cylinder head and valve cover seals; Fig. 8) because of their better tear and heat resistance. This trend has been assisted by the sharp rise in the number of diesel engines. ACM is increasingly displacing ECO for turbochar...
Kunststoffe international, 2005-11-21, Elastomers
...ss can be adapted to the particular load. This is a major aim for further improved polymers. Ester Rubbers (EVM, ACM, AEM): Acrylate rubber (ACM) Hytemp and NipolAR (Zeon) has become established in past years for large-area hot-oil seals (oil sump, engine bonnet and cylinder head-cover gaskets) because of the improved tear strength and heat resistance compared with NBR. The trend is accelerated by the growth of diesel engines. Zeon has expanded capacity at Louisville, KT/USA. ACM is increasingl...
Kunststoffe international, 2011-01-25, Appealing to (almost) all the Senses
...rades of high temperature polyacrylate elastomers (HTACM): These products offer the automobile industry new options for the development and production of high-performance component parts that are exposed to high temperatures and aggressive fluids. HyTemp AR214 was specially developed for gearbox oil cooler hoses and other rubber products that demand low compression set and raised sealing force. The application areas for HyTemp AR13FR are seals and sealing rings in the drive chain. In comparison ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.