Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Lucon" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
LUCON CP2100-KA02 | PC-CF |
LUCON CP5101F | (PC+ABS)-Z |
LUCON PN9009 | PPS-MF |
LUCON PS4200 | ABS-CF |
LUCON TR1000 | PMMA-Z |
LUCON CP-6052 | (PC+ABS)-Z |
LUCON CP-6062EX | (PC+ABS)-Z |
LUCON CP-6067 | PC-CF... |
LUCON CP-6080LP | PC-CF... |
LUCON PN9008 | PPS-MF |
LUCON PO-6062 | PPO-(CF+GF)... |
LUCON PO-6063 | PPO-(CF+GF)... |
LUCON PS-6080EX | ABS... |
LUCON SP9306FL | PS-MF |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.